We have a weld on a cover that is cracking. I was wondering if anyone had any suggestions. The cover is 11x11.56x12.5 inches 0.090" thick AL 5052-H32. The two sides of the cover are welded onto the middle section with a .12 fillet weld ground down. The covers mount onto a machine that moves at 1g acceleration. There are two fasteners on each side of the cover (M4's) none on the top or bottom. We are seeing cracks along the weld at the tops of the covers. Any ideas ? I have requested, from the vendor, what they are using for a filler metal.