Oct 19, 2014 #1 t62 Mechanical Joined Sep 20, 2011 Messages 4 Location KW Can we make 2" tap and weld WELDOLET on 42" ASTM A A860 WPHY 60 TEE
Oct 21, 2014 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Yes. Upvote 0 Downvote