Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welding

Status
Not open for further replies.

JACKSTAN

Mechanical
Oct 5, 2005
21
What is minimum distance between shell circumferential weld and attached stiffening ring weld.
Is this value = 50 mm min.?
 
Replies continue below

Recommended for you

What is the original code of construction for the item?
 
I use 0.093 inches. Upon cooling, the weld sucks back the component by 33%, approximately. This means that the final gap between the components is 0.062 inches.

You need to gap the pieces being weld in order to achieve a good root penetration, hence "melt" to the parent material. Hope this helps.