Hi,
I’m looking at welding a 1.5" d barstock of nitronic 50. The material is Austenetic 209 SS. I’ve decided on a welding rod of 309L SS. From doing a carbon equivalency calculation it looks like this material should be preheated between 400 and 700F (calc from ASM #6 welding book). Post heat is going to be wrapped in blankets to cool slowly. My one concern is the possibility of sensitization (C = 0.06% in XM19) through the 850-450 range. Thoughts suggestions. The part cannot be put into a furnace as the length of the barstock in the end will exceed the furnace size. I suppose we could torch the part as well for a post heat, just like the pre heat. I’m thinking of keeping the part at the low end of the pre heat (400F) as I have also read the preheating stainless can cause more problems.
I’m looking at welding a 1.5" d barstock of nitronic 50. The material is Austenetic 209 SS. I’ve decided on a welding rod of 309L SS. From doing a carbon equivalency calculation it looks like this material should be preheated between 400 and 700F (calc from ASM #6 welding book). Post heat is going to be wrapped in blankets to cool slowly. My one concern is the possibility of sensitization (C = 0.06% in XM19) through the 850-450 range. Thoughts suggestions. The part cannot be put into a furnace as the length of the barstock in the end will exceed the furnace size. I suppose we could torch the part as well for a post heat, just like the pre heat. I’m thinking of keeping the part at the low end of the pre heat (400F) as I have also read the preheating stainless can cause more problems.