Hi,
1. Has anyone welded pipeline with tuboscope sleeve or any other sleeve/device that proctects internal coating while welding pipe?
2. So far, I have a WPS and PQR that is used for the pipe which is; 2"-8", API 5L x-42, x-52, x-60 materials and all butt welds, but with the addition of this sleeve, the manufacturer specified:
1. a specific range of travel speed
2. application of epoxy
3. using lowest heat setting possible
4. well ventilated welding space
5. max interpass temp. of 250 deg F
The above does not require re-qualification of the procedure right?
I mean, they can just be added to the existing procedure as "supplemental information" or "other" right?
Thank you.
1. Has anyone welded pipeline with tuboscope sleeve or any other sleeve/device that proctects internal coating while welding pipe?
2. So far, I have a WPS and PQR that is used for the pipe which is; 2"-8", API 5L x-42, x-52, x-60 materials and all butt welds, but with the addition of this sleeve, the manufacturer specified:
1. a specific range of travel speed
2. application of epoxy
3. using lowest heat setting possible
4. well ventilated welding space
5. max interpass temp. of 250 deg F
The above does not require re-qualification of the procedure right?
I mean, they can just be added to the existing procedure as "supplemental information" or "other" right?