Need to weld to a built up member, web is between 1/8" and 3/16" thick. Overall depth is 10.5", flanges 4" wide, 3/8" thick.
I am needing to weld a support for a channel to attach to it. Its approx. 1200 lb reaction. Would you do a continuous weld, or a stitch weld for an angle connection? I guess I am worried they will just burn thru the thin web.
My other option is a vertical plate to the flanges, and weld my channel to that. But I see that introducing more eccentricity to the beam.
Thoughts?
I am needing to weld a support for a channel to attach to it. Its approx. 1200 lb reaction. Would you do a continuous weld, or a stitch weld for an angle connection? I guess I am worried they will just burn thru the thin web.
My other option is a vertical plate to the flanges, and weld my channel to that. But I see that introducing more eccentricity to the beam.
Thoughts?