Is it possible to weld cast Stellite 12 to Inconel? The procedure we have received from our materials lab seems unreasonable. I haven't actually been able to find any information that this has been done successfully by anyone.

Thanks,
Kevin

 
Call Deloro Stellite. Holler back if you need a contact #
 