The fabricator wants to weld Stainless steel to A500 steel pipe. Can this be done?
 
Replies continue below

Recommended for you

I think there is a forum for welding and fabrication.
 
Stainless steel consumables can be used to weld carbon steel, so I can't see that St. Steel to A500 would be a problem.

You would have to assess if accelerated corrosion could be an issue.
 