I want to weld round bar (3/8" dia. H.R) to SCH. 40 pipe (1 1/4"), joining outside wall to outside wall so both pieces are running parrallel using FCAW.
My only concern is welding different diameter pieces together and getting the proper penetration.
1) Am I right in specifying a Flare V groove? If so,
2) Does AWS D1.1 apply? In particular Table 2.1 for selecting effective weld size and 4.10.5 qualifying this weld?
If not, can somebody point me in the right direction?
My only concern is welding different diameter pieces together and getting the proper penetration.
1) Am I right in specifying a Flare V groove? If so,
2) Does AWS D1.1 apply? In particular Table 2.1 for selecting effective weld size and 4.10.5 qualifying this weld?
If not, can somebody point me in the right direction?