I was told to plan out a new PQR to SMAW and GTAW SA-543 to SA-543 and also SA-543 to SA-541 Grade 5 forgings. The specs are for mat'ls already in the Q&T condition. What is the typical post weld on these? Is it typical to return to the Q&T condition? or simply stress relieve?
SA-543 principles are:
C=.2
Ni=2.75/3.90
Cr=1.5/2.0
Mo=.4/.6
Mg=.4/.7
SA-541 Grade 1 principles are:
C=.35
Ni=.4
Cr=.25
Mo=.1
Mg=.4/.9
What is suggested welding rod(s) and fillers for each combination??
Since the SA-541 has a much higher carbon (.35 max) than the SA-543 (.20 max) what issues should I be aware of or concerned about?
Thanks any advice or referrals are appreciated
SA-543 principles are:
C=.2
Ni=2.75/3.90
Cr=1.5/2.0
Mo=.4/.6
Mg=.4/.7
SA-541 Grade 1 principles are:
C=.35
Ni=.4
Cr=.25
Mo=.1
Mg=.4/.9
What is suggested welding rod(s) and fillers for each combination??
Since the SA-541 has a much higher carbon (.35 max) than the SA-543 (.20 max) what issues should I be aware of or concerned about?
Thanks any advice or referrals are appreciated