Aug 22, 2018 #1 stan000 Mechanical Joined Jul 31, 2014 Messages 121 Location CA Hello friends Welding process GTAW -P8 TO P8 - 308 L 1) IF I WANT TO USE 309 OR 316 FILLING MATERIAL DO I HAVE TO CHANGE WPS. 2) IF MY WELDER IS QUALIFIED FOR GMAW P1-P1 CAN HE WELD P8-P8 GTAW. regards stan
Hello friends Welding process GTAW -P8 TO P8 - 308 L 1) IF I WANT TO USE 309 OR 316 FILLING MATERIAL DO I HAVE TO CHANGE WPS. 2) IF MY WELDER IS QUALIFIED FOR GMAW P1-P1 CAN HE WELD P8-P8 GTAW. regards stan
Aug 23, 2018 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US You need to look this information up yourself in Section IX. Upvote 0 Downvote
Aug 23, 2018 #3 DekDee Petroleum Joined Mar 12, 2012 Messages 1,324 Location PH Couldn't agree more metengr. Stan, Open the code and read it - don't just come on here asking ridiculously basic questions. Upvote 0 Downvote
Couldn't agree more metengr. Stan, Open the code and read it - don't just come on here asking ridiculously basic questions.