Depending on the strength needed, there are different types of tee joint welds that can be used. The main types of Tee-Joints are:
a)Plain Tee-Joint,
b)Single Beveled Tee-Joint,
c)Double Beveled Tee-Joint,
d)Single-J Tee Joint,
e)Double-J Tee Joint.
For Welding Procedures Specifications(WPS) of plain Tee-Joint, A qualified WPS based on test piece with fillet welds could be used to welding of plain Tee-Joint.
So, if I want to weld beveled Tee-Joint(Single Beveled Tee-Joint, Double Beveled Tee-Joint, Single-J Tee Joint, Double-J Tee Joint), what type of test piece should be prepared and what tests should be conducted?
Thank you.Tee- Joint Types.jpg
 
Assuming you're working under ISO standards:
A beveled T-joint falls under butt welds (doesn't matter if it's full pen or partial pen, it's a butt weld).
For butt welds and in most cases, tensile, bend and impact testing is required. This means you'll have to perform a butt weld on plate, so you can provide the necessary test specimen. Usually for these kinds of joints, macro's are also recommended. This means you'll also have to do a pre-production weld test.

Make sure if you qualify fillet welds in a T-joint (one side a single layer, one side a multi layer), you take into account the double of the heat input if you're welding the first layer simultaneously. I try as much as possible to separate both tests (sl/ml), unless they are to be welded simultaneously in production as well.
 