Dear Mr. Metengr,
Please find below the requested informations:
C45 C /0,42-0,50 Si/0,40 Mn/0,50-0,80 P/0,45 S/0,45 - Cr/0,40 Mo/0,10 Ni/0,40
Rp/310 - 565 (Mpa) Rm/580 - 1050 (Mpa) -
Fe 430b equivalent to S275JR (EN10025):
C/0.22 Mn/1.5 P/0.045 S/0.045 N/0.009
Rp/275 (Mpa) Rm/410-560 (Mpa)
Thickness C45: 50mm
Thickness Fe430b: 16mm
(Fillet weld with SMAW process)
Best regards