I am reviewing welding procedures for a 304L Stainless Steel vessel. The design temperature of the vessel is -127C (-197F). According to ASME VIII, impact test is exempted for the base metal (UHA-51d). However, impact test for welding procedure qualification can not be exempted (UHA-51e). am I right?
If impact test is required for the welds, then the vendor shall provide the impact test value in the PQR. In this case, the supplementary essential variables are considered as Essential variable. Right? Please advice, thanks.
I am reviewing welding procedures for a 304L Stainless Steel vessel. The design temperature of the vessel is -127C (-197F). According to ASME VIII, impact test is exempted for the base metal (UHA-51d). However, impact test for welding procedure qualification can not be exempted (UHA-51e). am I right?
If impact test is required for the welds, then the vendor shall provide the impact test value in the PQR. In this case, the supplementary essential variables are considered as Essential variable. Right? Please advice, thanks.