Welding Plate to I beam

Status
Not open for further replies.

gasoperations

Mechanical
Nov 23, 2008
59
To increase the torsional resistance, I have to weld 10 mm thicjk plate to the flanges of an I beam to make it a box.

Could some one please advise how to specify the welding so as to prevent buckling during fabrication