So long at they are the same thickness at the weld end, this is not an issue. you will probably need a specific weld procedure and weld qualification tests as this could be an essential variable, but talk to welding engineer to see if your current welding procedures are valid or not. If not it's not a big cost to get ones that are.
Remember - More details = better answers
Also: If you get a response it's polite to respond to it.