Mohammad Saad
Mechanical
A crude distillation column has base metal SA-516 Gr-60. The top dome and 2 adjacent shell covers are hot-cladded with Monel (Alloy NO4400 as per ASME Section II, SB-127). The cladding is damaged due to corrosion, and it is decided to perform weld overlay of Monel SB-127 over corroded area (10m2), using ERNiCu-7 and GTAW. The manufacturing thickness of clad was 4.37~4.54 mm, while the remaining thickness of clad is 1.27~4.21 mm. The base CS metal is 21mm thick. I have been assigned a task to conduct research on the possible effects (distortion, etc.) of base metal (CS) due to the welding. Moreover, I need to study the best method and procedure of welding, and to ensure that the remaining cladding won't be affected by it. (There is no PWHT requirement for base metal as per drawings). If any of you could give your input and guide me to the best relevant resources to study, I would be obliged. Thanks in advance.