Jegan Thiyagarajan
Petroleum
As per Sec IX QW-360; P.No & F.no is not an essential variable for welding operator - Machine welding
My concern is we have different procedure qualification (WPS) in our database. If welding operator qualified for Sl.No.1 below can weld Sl.No. 2 to 7 within the limits of the essential variables QW-361.2.
Sl.No. 1, AISI4130 + Inconel 625
Sl.No. 2, A106 + Inconel 625
Sl.No. 3, A106 + SS316L
Sl.No. 4, SA234 WP22 Cl 3+SS 347
Sl.No. 5, API 5L X65 PSL2 +SS 316L
Sl.No. 6, F22 + Inconel 625
Sl.No. 7, Alloy 625 + Inconel 625
Additional in QW-305 Paragraph 2 tells,
A welding operator qualified to weld in accordance with one qualified WPS is also qualified to weld in accordance with other qualified WPSs within the limits of the essential variables of QW-360.
Please help me.
My concern is we have different procedure qualification (WPS) in our database. If welding operator qualified for Sl.No.1 below can weld Sl.No. 2 to 7 within the limits of the essential variables QW-361.2.
Sl.No. 1, AISI4130 + Inconel 625
Sl.No. 2, A106 + Inconel 625
Sl.No. 3, A106 + SS316L
Sl.No. 4, SA234 WP22 Cl 3+SS 347
Sl.No. 5, API 5L X65 PSL2 +SS 316L
Sl.No. 6, F22 + Inconel 625
Sl.No. 7, Alloy 625 + Inconel 625
Additional in QW-305 Paragraph 2 tells,
A welding operator qualified to weld in accordance with one qualified WPS is also qualified to weld in accordance with other qualified WPSs within the limits of the essential variables of QW-360.
Please help me.