Hi Friends,
Iam working on a project which consists of fixed cone roof newly built API 650 tanks, passed the hydro test requires some welding to be performed.
In the current condition, As per Fig.5.3a (roof-plate joint), lap joints of roof are externally fillet welded. Our design considered the same and test has been completed. As per its service requirement, the tank needs to be internally coated inclusive of its roof and accordingly the support structure was built as external.
In order to pass the holiday testing after internal coating on the roof, the open lap joints shall not be open. Hence, My contractor is planning to do one pass welding on the roof joints to close the gap and also to avoid any crevice corrosion in the open area of the roof joint.
Since the tank has been already hydro tested, In accordance with 7.3.6.1 of 12th Edition of API 650, only non structural small attachments may be allowed to weld (please see the extract below). I need expert advice to achieve the same. Please help.
"7.3.6.1 This hydrostatic test of the tank shall be conducted before permanent external piping is connected to the
tank. Attachments to the shell defined in 5.8.1.1, located at least 1 m (3 ft) above the water level, and roof
appurtenances may be welded during the filling of the tank. After completion of the hydro-test, only non-structural
small attachments may be welded to the tank in accordance with 7.2.1.12."
Iam working on a project which consists of fixed cone roof newly built API 650 tanks, passed the hydro test requires some welding to be performed.
In the current condition, As per Fig.5.3a (roof-plate joint), lap joints of roof are externally fillet welded. Our design considered the same and test has been completed. As per its service requirement, the tank needs to be internally coated inclusive of its roof and accordingly the support structure was built as external.
In order to pass the holiday testing after internal coating on the roof, the open lap joints shall not be open. Hence, My contractor is planning to do one pass welding on the roof joints to close the gap and also to avoid any crevice corrosion in the open area of the roof joint.
Since the tank has been already hydro tested, In accordance with 7.3.6.1 of 12th Edition of API 650, only non structural small attachments may be allowed to weld (please see the extract below). I need expert advice to achieve the same. Please help.
"7.3.6.1 This hydrostatic test of the tank shall be conducted before permanent external piping is connected to the
tank. Attachments to the shell defined in 5.8.1.1, located at least 1 m (3 ft) above the water level, and roof
appurtenances may be welded during the filling of the tank. After completion of the hydro-test, only non-structural