Dear Material experts,

I have a pipe spool of SS321 being used for 1" riser along the flare stack.
I have short supply of material SS321, 1" pipe

Please suggest if I can use SS347 pipe spool available with me.
I need to weld the material as it has socket weld joints.

As per my study, E-347-16 welding rod is used for both, SS321 and SS347 material.

Please suggest if I can use SS347 pipe spool available with me.
 
Yes, indeed, the 347 pipe spool and weld rod will suffice in this application.
 
Should work fine. I see minimal risk.

= = = = = = = = = = = = = = = = = = = =