Good Day

M6 A2-70 bolts (ISO 3506) are tack (spot) welded using a 1x2mm fillet weld 6mm long onto a 316 SS plate to prevent rotation during bolt up. Is there a concern regarding the degradation of mechanical properties of the bolt for a service life of 30 years?

Any suggestions or further reading will be appreciated.

Kind Regards,
Richard
 
Welding on the bolt head? What size head? What welding process? Filler wire alloy? I would be concerned with corrosion resistance.
 
Yes, on the head

M6

I'll get back on that one

And this one too...

Yes, I'm concerned about chromium depletion in the heat affected zone
 