Dear Masters,

Will you please advise is it acceptable to weld A105 pipe nipples over A333 pipe?.

Thanks,
Energy2000
 
Replies continue below

Recommended for you

Yes, you can weld ASTM A 105 to ASTM A 333 provided you have a qualified welding procedure specification and certified welder.
 