Here are two suppliers of Micro-Tig and Micro-Plasma welding machines that I'm familiar with. Your requirements are well within the capabilities of either companies machines.
A good setup and working environment is essential in getting good micro welds. What little freehand work we accomplished an elbow support and stereo microscope were the essential aids.
I would check and see if either company has a video.