Assuming this was a report for a building in the US, you would be complying with AWS D1.1, Structural Welding Code-Steel. This code provides the discontinuities you noted and the allowed amount of each for particular types of welds. Based on the description, these are likely fillet welds with issues.
The link provided by BAretired gives pretty good graphics of the issues.