We qualified PQR inconel UNS 6625 weld to low temp Carbon Steel (A333 Gr 6). All mechanicate passed except Root bend test. The defect lack of fusion at boundary have appeared manny time. We try many time but still similar defect.
Would like give some information for your study:
Welding Consumable: Tech-Rod 112, ER NiCrMo-3 Techlloy
Heat input: 1.2-1.8 (Kj/mm)
Type bend: Root Bend
Jig Bend: 40 mm (4xt)
The picture for your refer