We have ASTM B705 N06625 and B366 N06625 in process modules that need to be welded. The tensile strength of the N06625 grade 1 material is 120 ksi. Please recommend what type of weld rod/filler metal should be used to weld the N06625 grade 1 material.
 
Replies continue below

Recommended for you

Though such alloys are not to be messed with, this is readily googled with good confidence, when looking at brochures from reknowned MFR's such as Special Metals, VDM, Haynes;

API RP 577 is also a good reference document. Review table D.3.
 