hello everybody. I have one question:
Is there problem at welding of Duplex 2205 with SA 304.
the vessel (130m2) is Duplex 2205 and his support beams is SA 304.
The temperature of the liquid is 90 °C


Thank you!
 
Replies continue below

Recommended for you

What does the Outokumpu welding guide recommend for 2205 to 304 welds? Check there first.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
For your purpose type AWS 309 Mo with low carbon content,is better choice than SA 304.

REGARDS

luismarques
 
It's a dissimilar welding, but there are no particular problems. Just foreseen a buttering with 309 electrode on the 304 and then complete the welding.
these articles can give u some good advise
DISSIMILAR METAL WELDS AND WELD JOINT DESIGN FOR DUPLEX
STAINLESS STEELS


PRACTICAL GUIDELINES FOR THE FABRICATION OF DUPLEX STAINLESS STEELS