hello everybody. I have one question:
Is there problem at welding of Duplex 2205 with SA 304.
the vessel (130m2) is Duplex 2205 and his support beams is SA 304.
The temperature of the liquid is 90 °C
It's a dissimilar welding, but there are no particular problems. Just foreseen a buttering with 309 electrode on the 304 and then complete the welding.
these articles can give u some good advise
DISSIMILAR METAL WELDS AND WELD JOINT DESIGN FOR DUPLEX
STAINLESS STEELS