Dear David,If you are welding both sides (or can confirm UW-35 requirements): E = 0.7 no RT, E = 0.85 Spot RT, E = 1.0 Full RT
If you are welding one side (not able to satisfy UW-35): E = 0.65 no RT, E = 0.8 Spot RT, E = .90 Full RT
I would also suggest you take a look at App. 47.