Can you advise with the following if a welder is qualified to ASME IX SMAW 6G welding procedure IE 7018 electrodes . Is he qualified to weld butt of higher grade of consumable i.e. 10018 electrodes?
 
Replies continue below

Recommended for you

See QW-404.15 and QW-433 in Section IX.
 