Jul 18, 2005 #1 miyo Mechanical Joined Jul 18, 2005 Messages 12 Location IL What is the right method to weld steel pipes with inner concrete coating? How can I coat the welding area inside the pipe? Is there any information in the web? ty
What is the right method to weld steel pipes with inner concrete coating? How can I coat the welding area inside the pipe? Is there any information in the web? ty
Jul 18, 2005 #2 stanier Mechanical Joined May 20, 2001 Messages 2,442 Location AU Try http://www.tycowater.com.au and check out the Sintakote product. Upvote 0 Downvote