rudylyon57
Mechanical
- Apr 18, 2008
- 10
We have are welding an 8620 bushing (masked on all surfaces except bore during carburizing) into an A36 plate. The bushing is about 7.5" OD with a 1.25" wall and we are applying a fillet weld on the OD corner. That is, we are applying weld heat about 1" to 1.25" from the carburized surface. The problem is that we are cracking the parts. The bushing is being preheated to 400-500F before welding and the assembly is air-cooled. Any suggestions are greatly appreciated.