We tried to weld c45 Round Bar(400mm Dia) with IS2062 E350BR plate 32mm thk with E7018-1H4R with preheating 150Deg,but welding detatchment observed towards C45 side(photo attached).After welding PWHT at 620Deg C to be done.
We have some quantity of E12018-1H4R electrodes,can we use same.
Shall i require to change electrodes,parameters?/
krishh07
We have some quantity of E12018-1H4R electrodes,can we use same.
Shall i require to change electrodes,parameters?/
krishh07