Aug 12, 2003 #1 marshell Mechanical Joined Jun 6, 2003 Messages 64 Location US Is it possible to get a good weld with AR500 (aka Wearalloy 500) to AR500, and AR 500 to A-36 Steel? I have been told that with the carbon content of AR500 at .30 it will be difficult. Thanks in advance, Marshall
Is it possible to get a good weld with AR500 (aka Wearalloy 500) to AR500, and AR 500 to A-36 Steel? I have been told that with the carbon content of AR500 at .30 it will be difficult. Thanks in advance, Marshall
Aug 12, 2003 1 #2 Goahead Aerospace Joined Jul 13, 2003 Messages 625 Location IL Contact the source at: http://www.fordsteel.com/wear_plates_bars.htm They will tell you how to weld. http://www.welding-advisers.com/ Upvote 0 Downvote
Contact the source at: http://www.fordsteel.com/wear_plates_bars.htm They will tell you how to weld. http://www.welding-advisers.com/
Aug 12, 2003 #3 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US AR500 can be readily welded to A-36 with E7018 electrodes with moderate preheat as thickness increases or ambient temperature declines below 50 F. Upvote 0 Downvote
AR500 can be readily welded to A-36 with E7018 electrodes with moderate preheat as thickness increases or ambient temperature declines below 50 F.