Good day all,
a little help is required in resolving a problem.
According to asme ix - Group numbers is a supplementary variable. To my understanding its a requirement for CVN.
However - our WPS Procedure A 106 - have P1 Group 1 which uses GTAW ER70S-6 and E 7018 H4R and no CVN was a used to qualify the procedure.
During my research, i realised that the same electrodes can be used to weld API 5L X 60 - P number 1 Group # 2.
My question is - do i need to do a new WPS to weld this API 5L X 60 pipe????
Thanks in advance
a little help is required in resolving a problem.
According to asme ix - Group numbers is a supplementary variable. To my understanding its a requirement for CVN.
However - our WPS Procedure A 106 - have P1 Group 1 which uses GTAW ER70S-6 and E 7018 H4R and no CVN was a used to qualify the procedure.
During my research, i realised that the same electrodes can be used to weld API 5L X 60 - P number 1 Group # 2.
My question is - do i need to do a new WPS to weld this API 5L X 60 pipe????
Thanks in advance