My question relates to removing (through grinding) 1st gear on a mainshaft, removing a 2nd gear with a lower ration from another gearbox, and welding it onto the original shaft.
I had originally hoped I could do this by tig welding, cooling, repeat. This would have avoided annealing shaft and gear.
However, trying this out has proved this to be easier said than done, and to get a decent fillet means the shaft and gear are softened.
This leaves me with a question, can the shaft, once welded to this new gear be heat treated back to something close to original hardness?
The application is a low mileage dirt track car, normally run in one gear, but it needs a "gate" gear to take it to the first bend, hence the fitting of a lower second gear in place of the original 1st.
Thanks,
Huw
I had originally hoped I could do this by tig welding, cooling, repeat. This would have avoided annealing shaft and gear.
However, trying this out has proved this to be easier said than done, and to get a decent fillet means the shaft and gear are softened.
This leaves me with a question, can the shaft, once welded to this new gear be heat treated back to something close to original hardness?
The application is a low mileage dirt track car, normally run in one gear, but it needs a "gate" gear to take it to the first bend, hence the fitting of a lower second gear in place of the original 1st.
Thanks,
Huw