Hello Everybody:
Appreciate if anybody could help me here as I am not too proficient in welding.
(1) I have a AL6XN (P45) material to Suplex Duplex (P10H), Will it be a good to weld using filler wire Er NiCrMo-3.
(2) I have a procedure to weld P45 to P45 & my qualification range is P1 thru P11, P34 & P4X. Am I good to weld P45 to P10H
Thank you
Bret
Appreciate if anybody could help me here as I am not too proficient in welding.
(1) I have a AL6XN (P45) material to Suplex Duplex (P10H), Will it be a good to weld using filler wire Er NiCrMo-3.
(2) I have a procedure to weld P45 to P45 & my qualification range is P1 thru P11, P34 & P4X. Am I good to weld P45 to P10H
Thank you