Hi
I need to know proper welding consumable for welding A514 to A516. unfortunatley I did n't find anything about this on the internet.
Can you help me guys?[smile]
 
The internet is not a welding engineer.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
go to ASME IX and qualify your welding procedure.


luis marques
 
Use a low hydrogen SMAW electrode or other low hydrogen welding process. More information is required to be more definitive.

Best regards - Al
 
Don't be shy to call your welding supplier. Often they are are great resources when determining filler metals.

We weld A517 with SMAW 11018, that might be a good starting point if you don't need a high volume. Otherwise the Lincoln sells a ultracore 121K3C-H that might work in your application.

As already mentioned we don't have many details on what your application is, but these might be a good starting point.

If you gave us more information we could help more. PWHT, Thickness, impacts?

Regards
 