I need to weld A350-LF3 with a restriction of no FCAW. I am having a problem in finding consumables - EN-Ni3.
Does anyone see any reason why I could not qualify a PQR using 309 consumables? I already have a PQR qualified for welding LF3 to P8.
Any help would be appreciated.
Does anyone see any reason why I could not qualify a PQR using 309 consumables? I already have a PQR qualified for welding LF3 to P8.