May 27, 2019 #1 PipeliningExpert Petroleum Joined Dec 31, 2013 Messages 2 Location US Is it ok Welding A105 forged fittings to 5L GR-X65 pipe or should use A694 GR-F65 weldolets, nipolet, etc.
Is it ok Welding A105 forged fittings to 5L GR-X65 pipe or should use A694 GR-F65 weldolets, nipolet, etc.
May 27, 2019 #2 LittleInch Petroleum Joined Mar 27, 2013 Messages 23,016 Location GB With a proper welding spec this shouldn't be an issue so long as the fitting is the correct thickness for the pressure. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
With a proper welding spec this shouldn't be an issue so long as the fitting is the correct thickness for the pressure. Remember - More details = better answers Also: If you get a response it's polite to respond to it.
May 28, 2019 Thread starter #3 PipeliningExpert Petroleum Joined Dec 31, 2013 Messages 2 Location US Thank you LittleInch, I normally prefer to use ASTM A694 forged fittings with a grade to match that of main pipe grade at least to the first flange. In cases where a nipple is required, I do not know if they make nipples also to Grade X65. Upvote 0 Downvote
Thank you LittleInch, I normally prefer to use ASTM A694 forged fittings with a grade to match that of main pipe grade at least to the first flange. In cases where a nipple is required, I do not know if they make nipples also to Grade X65.
May 28, 2019 #4 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US This is done quite often due to availability of sourcing small diameter F65 and Y65 forging and fittings. Upvote 0 Downvote
This is done quite often due to availability of sourcing small diameter F65 and Y65 forging and fittings.