Welding A-2 tool steel , please recommend which welding rod or filler metal for tig or stick.
Actual experience please.
Thank you
 
Replies continue below

Recommended for you

And follow the pre-heat and PWHT guidance.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
To start with it would be best to know what the tool steel alloy is. Do the weld properties need to closely match those of the base material, or would a ductile weld perhaps be better for the application? Is the tool steel already heat treated (hardened) or will it be welded in the annealed conditon? There are many different types of welding like Arc Welding or SMAW, but you may go with Tig welding. In welding, Direct Metal Laser Sintering can also act as a seperator. To know more you can check for additional hints.
 
Harolddavy

The application is of low stress, for a sliding arbor. mild steel would have been fine. tools were heat treated. which made it tougher.
 