we are having a problem welding 4140 square bar to mild plate. we have tried 9598 and similar but with no success. the part will be in operation for a month or so then split. the 4140 is 2x2 sq.bar and a 5" x 1-1/4 flat bar is welded perpendicular to it so the 5" f.b. is welded to the 12' 4140 bar. If anyone has experiance making this stick please fill me in.