I'm looking for suggestions on making a successful weld in 410 material. I recently completed a test plate in 1" thick material which was welded using the SMAW process with a 400 F preheat, followed by a 600 F DHT and a 1400 F PWHT but unfortunately we had problems with very coarse grains resulting in mechanical issues.
It has been suggested that we change our PWHT procedure from a ramp up rate of 400F / hr, to increasing the temperature as quick as possible to 1000 F, hold at 1000 F for an hour and ramp up to 1400 F at 400 F/hr and cooling from a 1000 F to around 600 F fairly quickly. Any thoughts?
Thanks,
John
It has been suggested that we change our PWHT procedure from a ramp up rate of 400F / hr, to increasing the temperature as quick as possible to 1000 F, hold at 1000 F for an hour and ramp up to 1400 F at 400 F/hr and cooling from a 1000 F to around 600 F fairly quickly. Any thoughts?
Thanks,
John