Ihave a local shop that is haing severe welding problems while welding 2205 SS/2205 SS and 2205 SS/340lSS. The welds are supposed to be strenght welds, no code. The equipment has been in use several years and is very dirty and coated with polymer. Best effort cleaning
appears to have no effect on the welding problems. I am trying to get the welding spec and what has been tried. I made some welds on this equipment some 20 yrs ago using Cronotron 3880 and they are still holding. The question is has anyone tried any different consumable for this type weld and maybe a little on procedure.
Thanks
appears to have no effect on the welding problems. I am trying to get the welding spec and what has been tried. I made some welds on this equipment some 20 yrs ago using Cronotron 3880 and they are still holding. The question is has anyone tried any different consumable for this type weld and maybe a little on procedure.