I'm in the process of designing some piping modifications for a replacement pump. I'm somewhat limited, in the vertical dimension, for my discharge pipe and fittings. Is it possible to weld a 2" pipe into the side of a A234 WPB 4" x 3" reducer without sacrificing the integrity of the reducer? Essentially what I would like to do is turn my 4" x 3" reducer into a 4" x 3" reducgin tee with a 2" side outlet. The reducer length is standard at 4".
Otherwise, I will install a 4" x 2" outlet reducing tee downstream of the 4" x 3" reducer.
Jonathan Ives
Project Engineer
Transalta, Alberta Thermal Plants
Duffield, Alberta
Otherwise, I will install a 4" x 2" outlet reducing tee downstream of the 4" x 3" reducer.