brianmiller8002
Materials
- Apr 26, 2009
- 1
We are currently welding 1.5" 4140 material together with a preheat of only 150F. The part is stress relieved (often not until the next day or even longer). Then the inside diameter is slightly machined and the unit is sent to NDT (Mag Particle). We were having failures of roughly 1 out of 11 at NDT where we simply machined out the bad area and repeated the welding procedure. Well, most recently we had a batch sit after the weld for over a week before it was stress relieved and we experienced a 90% failure rate without changing any other variables as far as we can tell. Can snyone tell us if the amount of time before stress relief and after weld is a factor? What other variables are key factors? What are other things to consider in this application? Are we preheating enough?
Thanks!