Guys

Need your help, I will be conducting WQT by next week with our WPS that is qualified for API X60 PIPE and A707 CL3 L5 FLANGE. API X60 IS P1 GR2 and A707 CL3 L5 FLANGE does not have Pno assignment as per ASME SEC 1X

question? can we have substitution in WQT. instead of A707 CL3 L5 FLANGE we will used API X60 PIPE because it has the same min 75 KSI tensile strength. Also cost of material for A707 flange is expensive..


Thank you
 
Replies continue below

Recommended for you

QW-423.2 - "Metals used for welder qualification conforming to national or international standards or specifications may be considered as having the same P-Number as an assigned metal provided it meets the MECHANICAL and CHEMICAL requirements of the assigned metal. The base metal specification and corresponding P-Number shall be recorded on the qualification record."
 