QW-408.8 of ASME IX states that the omssion of an inert backing gas calls for requalification if used in the WPQ. If the welder was tested on a pipe with an inert gas backing, is he qualified for butt welding plate single sided, complete penetration, without any backing?
 
That's an easy one "No". A complete penetration single sided weld does not comply with with the text of QW-408.8
"Requalification is not required when welding a single welded butt joint with a backing strip or a double-welded butt joint or a fillet weld."
 
However, if the welder cleans up the 2nd side [grinder, air-arc] and welds on that side, he is qualified. Used the 1st side weldmetal as his backing, Metal backing can be substituted for gas backing.
 
Thank you very much. You just confirmed what i thought it should be.
 