Hi,
1. I understand that a welder qualified to weld an F6 filler metal is automatically qualified to weld F5 -F1, does it matter if it's the same or a different process? example, a welder qualified with TIG ER-70S-6, can the welder weld a 7018 and/or 7010 electrode SMAW?
2. If the welder is going to weld a 4130 (unassigned) to an A106 B (P1) in production, does the welder's qualification test have to be on a 4130 to P1? or can a welder test with a P1 to P1 and weld the above?
Thank you for your help and input.
As much as possible, do it right the first time...
1. I understand that a welder qualified to weld an F6 filler metal is automatically qualified to weld F5 -F1, does it matter if it's the same or a different process? example, a welder qualified with TIG ER-70S-6, can the welder weld a 7018 and/or 7010 electrode SMAW?
2. If the welder is going to weld a 4130 (unassigned) to an A106 B (P1) in production, does the welder's qualification test have to be on a 4130 to P1? or can a welder test with a P1 to P1 and weld the above?
Thank you for your help and input.
As much as possible, do it right the first time...