Dec 11, 2014 #1 cjgrass Industrial Joined Apr 8, 2013 Messages 34 Location US Can a welder that has qualified on 8 5/8"OD x 0.500" pipe SVG 6G position using E8010-P1 for bead and hot pass and E8018-C3 fill and cap be used to weld A572Gr50 1/2" plate SVG with backing using only E7018-1 in the 3G position? Thanks
Can a welder that has qualified on 8 5/8"OD x 0.500" pipe SVG 6G position using E8010-P1 for bead and hot pass and E8018-C3 fill and cap be used to weld A572Gr50 1/2" plate SVG with backing using only E7018-1 in the 3G position? Thanks
Dec 11, 2014 #2 aburafdi Materials Joined Feb 13, 2012 Messages 48 Location ID As the welder use F4 for his qualification (with backing of F3), yes he can weld using F4 with backing. Regards, AR Upvote 0 Downvote
As the welder use F4 for his qualification (with backing of F3), yes he can weld using F4 with backing. Regards, AR